Subject: Polishing contact area By: Stagolee (IP: 212.159.47.*) Written on: 09-09-2005 15:43
Hi
I noticed that the heatsink contact area shown on the site is highly polished. Is that something you can do yuorself? Is it recommended? Would Brasso or Silvo be the right way?
Stag
Replies:
By: Tillmann (IP: 146.140.7.*) Written on: 13-09-2005 15:28
Hi,
yes, this is possible. The procedure is known as heatsink lapping.